This chapter discusses material-related problems associated with coal-fired burners. It explains how high temperatures affect heat-absorbing surfaces in furnace combustion areas and in the convection pass of superheaters and reheaters. It describes how low-NOx combustion technology, intended to reduce NOx emissions, accelerates tube wall wastage. It also covers circumferential cracking in furnace waterwalls, thermal fatigue cracking induced by waterlances and water cannons, superheater-reheater corrosion, and erosion in fluidized-bed boilers.