This chapter describes the corrosion behavior of beryllium in gaseous atmospheres, including oxygen, nitrogen, carbon dioxide, and carbon monoxide. It also discusses the development of high-temperature corrosion-resistant beryllium alloys.

You do not currently have access to this chapter.
Don't already have an account? Register

Kenneth A. Walsh, David L. Olson, Alfred Goldberg, Warren Haws, High-Temperature Corrosion of Beryllium and Beryllium Alloys, Beryllium Chemistry and Processing, By Kenneth A. Walsh;Edited By Edgar E. Vidal, Alfred Goldberg, Edward N.C. Dalder, David L. Olson, Brajendra Mishra, ASM International, 2009, p 485–492, https://doi.org/10.31399/asm.tb.bcp.t52230485