Beryllium is an important additive in the production of amorphous metal alloys, achieving low density and high strength. It also plays a role in amorphous alloys that can be slowly cooled and still retain their amorphous structure. This chapter provides information on the development of amorphous alloys that contain beryllium and the applications for which they are suited.

You do not currently have access to this chapter.
Don't already have an account? Register

Loren A. Jacobson, Robert Hanrahan, Amorphous Alloys That Contain Beryllium, Beryllium Chemistry and Processing, By Kenneth A. Walsh;Edited By Edgar E. Vidal, Alfred Goldberg, Edward N.C. Dalder, David L. Olson, Brajendra Mishra, ASM International, 2009, p 145–149, https://doi.org/10.31399/asm.tb.bcp.t52230145