This chapter discusses the properties and applications of beryllium intermetallic compounds. It describes the crystal structure of key beryllides, the metals they contain, and important properties such as high-temperature strength, thermal conductivity and expansion, oxidation resistance, and density. It explains how beryllide intermetallics are formed using sputter deposition, diffusion, and powder metal methods.

You do not currently have access to this chapter.
Don't already have an account? Register

Christopher Dorn, Loren A. Jacobson, Gilbert London, Beryllium Intermetallic Compounds, Beryllium Chemistry and Processing, By Kenneth A. Walsh;Edited By Edgar E. Vidal, Alfred Goldberg, Edward N.C. Dalder, David L. Olson, Brajendra Mishra, ASM International, 2009, p 131–144, https://doi.org/10.31399/asm.tb.bcp.t52230131