Abstract

This chapter describes some of the chemical processes that have been developed to extract beryllium from different types of ore. It covers the Kjellgren-Sawyer sulfate method, the Degussa method, Copaux-Kawecki fluoride extraction, solvent extraction, and leaching and settling. It also provides information on electrolytic extraction and the use of electrorefining.

You do not currently have access to this chapter.
Don't already have an account? Register

Kenneth A. Walsh, Edgar E. Vidal, Brajendra Mishra, Extractive Metallurgy, Beryllium Chemistry and Processing, By Kenneth A. Walsh;Edited By Edgar E. Vidal, Alfred Goldberg, Edward N.C. Dalder, David L. Olson, Brajendra Mishra, ASM International, 2009, p 71–92, https://doi.org/10.31399/asm.tb.bcp.t52230071