Abstract

This chapter is a detailed account of the tensile testing procedure used for evaluating metals and alloys. The discussion covers the stress-strain behavior of metals determined by tensile testing, properties determined from testing, test machines for measuring mechanical properties, and general procedures of tensile testing. Three distinct aspects of standard test methods for tension testing of metallic materials are discussed: test piece preparation, geometry, and material condition; test setup and equipment; and test procedure.