Abstract

This chapter discusses the operating mechanism, applications, advantages, and limitations of Brinell hardness testing, Rockwell hardness testing, Vickers hardness testing, Scleroscope hardness testing, and microhardness testing. In addition, the general precautions and selection criteria to be considered are described and details of equipment setup provided.

You do not currently have access to this chapter.
Don't already have an account? Register

Hardness Testing, Inspection of Metals: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2013, p 85–116, https://doi.org/10.31399/asm.tb.imub.t53720085