This chapter is intended to identify materials, processes, and designs that will lead to great advances in powder-binder forming technologies. It discusses some of the structures obtained through these advances in powder-binder technologies such as binder jetting and extrusion-based additive manufacturing, including bound-metal deposition and fused-filament fabrication: oxidation-resistant high-temperature alloys, anisotropic structures, submicrometer-scale structures, surface hard materials, and artist metallic clays. Some of the advances discussed include the developments in process involving plastics, emulsions, ceramics, and porous structures and foams. Improvements in the design processes have led to the development of functional structures, controlled porosity, and bioinspired structures.

You do not currently have access to this chapter.
Don't already have an account? Register

Opportunities for Powder-Binder Forming Technologies, Binder and Polymer Assisted Powder Processing, By Randall M. German, Animesh Bose, ASM International, 2020, p 251–260, https://doi.org/10.31399/asm.tb.bpapp.t59290251

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal