This chapter provides details on powder-binder processing for three materials, namely precipitation-hardened 17-4 PH stainless steel, cemented carbides, and alumina. The types of powders, binders, feedstock, shaping processes, debinding, sintering cycles, compositions, microstructure, distortion, postsintering treatments, and mechanical properties are presented for each. The shaping options include powder-binder approaches such as binder jetting, injection molding, extrusion, slip and slurry casting, centrifugal casting, tape casting, and additive manufacturing. Sintering options are outlined with respect to attaining high final properties.

You do not currently have access to this chapter.
Don't already have an account? Register

Case Studies of Powder-Binder Processing Practices, Binder and Polymer Assisted Powder Processing, By Randall M. German, Animesh Bose, ASM International, 2020, p 201–249, https://doi.org/10.31399/asm.tb.bpapp.t59290201

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal