Abstract

This article discusses the role of alloying in the production and use of common refractory metals, including molybdenum, tungsten, niobium, tantalum, and rhenium. It provides an overview of each metal and its alloys, describing the compositions, properties, and processing characteristics as well as the effect of alloying elements. It also discusses strengthening mechanisms and, where appropriate, corrosion behavior.

You do not currently have access to this chapter.
Don't already have an account? Register

Refractory Metal Alloys, Alloying: Understanding the Basics, Edited By J.R. Davis, ASM International, 2001, p 308–336, https://doi.org/10.31399/asm.tb.aub.t61170308