A major effort in the development of thermal spray applications has been the improvement of process reliability and predictability in response to process changes. The ability to model a process is a prerequisite to understanding and controlling it. This article provides an overview of thermal spray process modeling, as it applies to the engineering of new thermal spray equipment and coating development.