High-velocity oxyfuel (HVOF)-applied thermal spray coatings are viable candidates for replacement of hard chrome in numerous applications. HVOF thermal spraying can be used to deposit both metal alloy and cermet coatings that are dense and highly adherent to all the commonly used base metals in airframe structures. This article summarizes the results of materials and component testing. It also presents a cost/benefit analysis of HVOF WC/17Co and WC/10Co4Cr coatings on aircraft landing gear components.