Thermal and Environmental Barrier Coatings (TBCs/EBCs) for Turbine Engines

By
Rogerio S. Lima
Rogerio S. Lima
National Research Council of Canada (NRC)
Search for other works by this author on:
;
Dongming Zhu
Dongming Zhu
National Aeronautics and Space Administration (NASA)
Search for other works by this author on:
;
Li Li
Li Li
Praxair Surface Technologies
Search for other works by this author on:
Published:
2013
Page range:
270 - 279
Publication history
February 13, 2013

Abstract

This article presents a summary of the current and new materials and processing techniques for thermal barrier coatings (TBCs) and environmental barrier coatings (EBCs). Different thermal spraying and postspraying processing techniques are required to produce coatings with optimal performance. For TBCs and EBCs, the elastic modulus, mechanical strength, and toughness values are extremely important in predicting failure behavior under stress and strain conditions, mainly for modeling purposes. Sand and/or volcanic ash particles are molten in the hot zones of turbines and deposited over TBCs and EBCs. They form calcium-magnesium-aluminosilicate (CMAS) glassy deposits.

You do not currently have access to this content.
Don't already have an account? Register

Rogerio S. Lima, Dongming Zhu, Li Li, 2013. "Thermal and Environmental Barrier Coatings (TBCs/EBCs) for Turbine Engines", Thermal Spray Technology, Robert C. Tucker, Jr.