This article presents a summary of the current and new materials and processing techniques for thermal barrier coatings (TBCs) and environmental barrier coatings (EBCs). Different thermal spraying and postspraying processing techniques are required to produce coatings with optimal performance. For TBCs and EBCs, the elastic modulus, mechanical strength, and toughness values are extremely important in predicting failure behavior under stress and strain conditions, mainly for modeling purposes. Sand and/or volcanic ash particles are molten in the hot zones of turbines and deposited over TBCs and EBCs. They form calcium-magnesium-aluminosilicate (CMAS) glassy deposits.

You do not currently have access to this chapter.
Don't already have an account? Register

Rogerio S. Lima, Dongming Zhu, Li Li, 2013. "Thermal and Environmental Barrier Coatings (TBCs/EBCs) for Turbine Engines", Thermal Spray Technology, Robert C. Tucker, Jr.

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal