This article is a brief guide to information sources on thermal spray technology. The sources provided by ASM International and the Thermal Spray Society (TSS) include magazines and journals as well as reference books, including the ASM Handbook series, conference proceedings, newsletters, education courses, and videos. The article provides information on the specifications, standards, and quality control for coatings.

You do not currently have access to this chapter.
Don't already have an account? Register

R.C. Tucker, Jr., 2013. "Guide to General Information Sources", Thermal Spray Technology, Robert C. Tucker, Jr.