Abstract

The use of renewable energy has grown strongly in all end-use sectors such as power, heat, and transport. This article describes thermal spray applications that improve efficiency, lower maintenance costs, and prolong operational life in the renewable energy technologies, including wind power, hydro power, biomass and biofuels, solar energy, and fuel cells.

You do not currently have access to this chapter.
Don't already have an account? Register

Robert Vassen, Georg Mauer, Renewable Energy Applications, Thermal Spray Technology, Vol 5A, ASM Handbook, Edited By Robert C. Tucker, Jr., ASM International, 2013, p 318–321, https://doi.org/10.31399/asm.hb.v05a.a0005708