Thermal Spray Applications in the Paper Production Industry[1]
-
Published:2013
Abstract
Thermal spray coatings, along with certain proprietary sealants, are widely used in the paper manufacturing industry for corrosion and wear resistance and to impart special surface characteristics. This article discusses the steps involved in the paper manufacturing process. Most modern papermaking machines are based on variations of the Fourdrinier machine. The article describes four operational sections of the machine: forming, press, drying, and calendar. It provides an overview of the machine components where thermal spray coatings are used, namely digesters, blow tanks, suction roll, center press rolls, yankee dryer rolls, calendar rolls, doctor/scalping blades, and cutting equipment.
Sign in
ASM members
Member Sign InMitchell R. Dorfman, Atin Sharma, Thermal Spray Applications in the Paper Production Industry, Thermal Spray Technology, Vol 5A, ASM Handbook, Edited By Robert C. Tucker, Jr., ASM International, 2013, p 328–331, https://doi.org/10.31399/asm.hb.v05a.a0005743
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.