Abstract

Significant expansion of thermal spray technology occurred with the invention of plasma spray, detonation gun, and high-velocity oxyfuel (HVOF) deposition technologies. This article provides a brief history of the major initiating inventions/developments of thermal spray processes. It provides information on feedstock materials developed for specific thermal spray processes.

You do not currently have access to this chapter.
Don't already have an account? Register

R.C. Tucker, Jr., A Brief History of the Development of Thermal Spray Processes and Materials, Thermal Spray Technology, Vol 5A, ASM Handbook, Edited By Robert C. Tucker, Jr., ASM International, 2013, p 348–350, https://doi.org/10.31399/asm.hb.v05a.a0005713