Thermal Spray Technology
Volume 5A provides an introduction to thermal spray technology including plasma spray, high velocity oxy-fuel, and detonation gun deposition. It explains how each process works and the types of coating materials typically used. It also addresses critical application issues, including substrate requirements, surface preparation, bonding agents, adhesion, and uniformity, and their effect on surface properties, wear, corrosion, and thermal barrier performance. The volume also provides practical information on how to test and analyze thermal spray coatings and it presents several examples of how thermal spray technology is being used. For information on the print version of Volume 5A, ISBN: 978-1-61503-996-8, follow this link.
Download citation file:
Close
Table of Contents
-
Introduction to Thermal Spray Technology and Surface Engineering
-
Introduction to Thermal Spray TechnologyByR.C. Tucker, Jr.R.C. Tucker, Jr.Revising authorThe Tucker GroupSearch for other works by this author on:
-
Surface Engineering[1]ByR.C. Tucker, Jr.R.C. Tucker, Jr.The Tucker GroupSearch for other works by this author on:
-
-
Thermal Spray Processes and Coatings
-
Thermal Spray ProcessesByDaryl E. CrawmerDaryl E. CrawmerThermal Spray Technologies, Inc.Search for other works by this author on:
-
Cold Spray ProcessByJeganathan KarthikeyanJeganathan KarthikeyanRevising authorSearch for other works by this author on:
-
Coating Structures, Properties, and MaterialsByDaryl E. CrawmerDaryl E. CrawmerThermal Spray Technologies Inc.Search for other works by this author on:
-
Process Control and Control EquipmentByDaryl E. CrawmerDaryl E. CrawmerRevising authorThermal Spray Technologies Inc.Search for other works by this author on:
-
-
Consumables
-
Feedstock Material Considerations for Thermal SprayByNoppakun Sanpo;Noppakun SanpoSwinburne University of TechnologySearch for other works by this author on:Christopher C. BerndtChristopher C. BerndtSwinburne University of Technology and Stony Brook UniversitySearch for other works by this author on:
-
-
Precoating and Postcoating Processing
-
Health and Safety
-
Health and SafetyByDaryl E. CrawmerDaryl E. CrawmerRevising authorThermal Spray Technologies, Inc.Search for other works by this author on:
-
-
Testing and Characterization
-
Introduction to Testing and CharacterizationByDana RuckerDana RuckerRevising authorSiemensSearch for other works by this author on:
-
Testing of CoatingsByKen CouchKen CouchProtech Lab CorporationSearch for other works by this author on:
-
-
Existing and New Market Opportunities in Thermal Spray Applications
-
Introduction to Applications for Thermal Spray ProcessingByMitchell R. DorfmanMitchell R. DorfmanSulzer Metco (U.S.) Inc.Search for other works by this author on:
-
Corrosion Control for Marine- and Land-Based Infrastructure ApplicationsByShiladitya PaulShiladitya PaulTWI, Cambridge, United KingdomSearch for other works by this author on:
-
Corrosion and Wear Control for Industrial Applications[1]ByMitchell R. DorfmanMitchell R. DorfmanRevising authorSulzer Metco (U.S.) Inc.Search for other works by this author on:
-
Thermal Spray Coatings for Electrical and Electronic ApplicationsByAtin SharmaAtin SharmaSulzer Metco (U.S.) Inc.Search for other works by this author on:
-
Thermal and Environmental Barrier Coatings (TBCs/EBCs) for Turbine EnginesByRogerio S. Lima;Rogerio S. LimaNational Research Council of Canada (NRC)Search for other works by this author on:Dongming Zhu;Dongming ZhuNational Aeronautics and Space Administration (NASA)Search for other works by this author on:Li LiLi LiPraxair Surface TechnologiesSearch for other works by this author on:
-
Thermal Spray Technology Growth in Gas Turbine ApplicationsByMitchell R. Dorfman;Mitchell R. DorfmanSulzer Metco (U.S.) Inc.Search for other works by this author on:P. MeyerP. MeyerSulzer Metco (U.S.) Inc.Search for other works by this author on:
-
Abradable Thermal Spray Applications and TechnologyByScott WilsonScott WilsonSulzer Metco (Switzerland)Search for other works by this author on:
-
Automotive Coatings and ApplicationsByNoritaka MiyamotoNoritaka MiyamotoToyota Motor CorporationSearch for other works by this author on:
-
Biomedical Coatings Made by Thermal Spraying for Orthopaedic Joint ApplicationsByZongtao ZhangZongtao ZhangStryker Howmedica OsteonicsSearch for other works by this author on:
-
Protective Overlays and Coatings Used in Oil SandsByGary Fisher;Gary FisherAlberta Innovates—Technology FuturesSearch for other works by this author on:Tonya WolfeTonya WolfeAlberta Innovates—Technology FuturesSearch for other works by this author on:
-
Renewable Energy ApplicationsByRobert Vassen;Robert VassenForschungszentrum Jülich Institute of Energy and Climate Research (IEK-1)Search for other works by this author on:Georg MauerGeorg MauerForschungszentrum Jülich Institute of Energy and Climate Research (IEK-1)Search for other works by this author on:
-
Nuclear Industry Applications for Thermal SprayByKendall J. HollisKendall J. HollisLos Alamos National LaboratorySearch for other works by this author on:
-
Thermal Spray Applications in the Steel IndustryByCharles M. KayCharles M. KayASB Industries, Inc.Search for other works by this author on:
-
Thermal Spray Applications in the Paper Production Industry[1]ByMitchell R. Dorfman;Mitchell R. DorfmanRevising authorSulzer Metco (U.S.) Inc.Search for other works by this author on:Atin SharmaAtin SharmaRevising authorSulzer Metco (U.S.) Inc.Search for other works by this author on:
-
Printing Industry Applications[1]ByAtin SharmaAtin SharmaRevising authorSulzer Metco (U.S.) Inc.Search for other works by this author on:
-
Additional Applications in Thermal SprayByMitchell R. DorfmanMitchell R. DorfmanRevising authorSulzer Metco (U.S.) Inc.Search for other works by this author on:
-
-
Reference Information
-
Guide to General Information SourcesByR.C. Tucker, Jr.R.C. Tucker, Jr.Revising authorThe Tucker GroupSearch for other works by this author on:
-
A Brief History of the Development of Thermal Spray Processes and MaterialsByR.C. Tucker, Jr.R.C. Tucker, Jr.Revising authorThe Tucker GroupSearch for other works by this author on:
-