Vat polymerization (VP) is an additive manufacturing (AM), or three-dimensional (3-D) printing process in which 3-D objects are produced by hardening a liquid polymer into the desired shape. With the introduction of new materials and improvements in material properties, VP offers a good alternative for AM for low-volume production. This overview of the VP process begins with an introduction to two main processes of VP, namely stereolithography apparatus and digital light processing, and then moves on to discuss the characteristics of the feedstocks used as well as their selection criteria. The article then covers safety issues associated with feedstock...