Induction hardening of steel components is the most common application of induction heat treatment of steel. This article provides a detailed account of electromagnetic and thermal aspects of metallurgy of induction hardening of steels. It describes induction hardening techniques, namely, scan hardening, progressive hardening, single-shot hardening, and static hardening. The article discusses the techniques used to control the heat pattern, and provides a brief review of quenching techniques used in the induction hardening. It provides guidelines for selecting the frequency and power for induction hardening, and describes common methods for measuring case depth, such as optical and microhardness, and surface hardness. It provides information on some complications and ambiguities associated with these measurements. The article also discusses the commonly used non-destructive testing methods, namely, magnetic particle testing, ultrasonic testing, and eddy current testing to evaluate induction-hardened components.

You do not currently have access to this chapter.
Don't already have an account? Register

Valery Rudnev, Gregory A. Fett, Arthur Griebel, John Tartaglia, 2014. "Principles of Induction Hardening and Inspection", Induction Heating and Heat Treatment, Valery Rudnev, George E. Totten

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal