Abstract

Melting with induction crucible furnaces (ICFs) is a well-established and reliable technology, and their maintenance must be performed at regularly scheduled intervals to ensure safe operation. This article discusses monitoring of the refractory lining, and presents an overview of the various wear-indication methods, namely, manual checks, ground leakage indication, evaluation of electrical values of the furnace, and temperature measurement. It also presents the working principle, physical restrictions, limitations, and remarks on these methods.

You do not currently have access to this chapter.
Don't already have an account? Register

Manfred Hopf, 2014. "Operating Safety of Induction Melting Furnaces", Induction Heating and Heat Treatment, Valery Rudnev, George E. Totten