Induction processes for melting and heating of metals belong to the high-energy-consuming industrial processes, and continuous improvement of energy efficiency of competitive melting and heating technologies is of increasing interest. This article discusses the energy demand of various melting processes and the improvements in the efficiency of melting processes in induction crucible furnaces. It provides energetic and ecological comparisons of different furnaces for melting of cast iron and aluminum. The article also describes the energy and power management of induction melting processes.

You do not currently have access to this chapter.
Don't already have an account? Register

Egbert Baake, Bernard Nacke, Energy and Environmental Aspects of Induction Melting Processes, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 548–554, https://doi.org/10.31399/asm.hb.v04c.a0005908

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal