Induction heating system control is straightforward after the design and application of the coil and power supply required for the job. This article provides an overview of the basic components of an induction heating system, including a machine controller (computer or programmable logic controller), interface wiring, an operator interface, and safety controls. It also provides information on programming devices and temperature controllers, such as manual, auto, and auto-manual temperature controllers.