The shafts on two centrifugal pumps failed during use in a petroleum refinery. Light optical microscopy and scanning electron microscopy were used to analyze the damaged materials to determine the cause of failure. The results showed that one shaft, made of duplex stainless steel, failed by fatigue fracture, and the other, made of 316 austenitic stainless steel, experienced a similar fracture, which was promoted by the presence of nonmetallic inclusion particles.

You do not currently have access to this chapter.
Don't already have an account? Register

Cássio Barbosa, Jôneo Lopes do Nascimento, José Luiz Fernandes, Ibrahim de Cerqueira Abud, 2019. "Failure Analysis of Two Stainless Steel Based Components Used in an Oil Refinery", Handbook of Case Histories in Failure Analysis, Larry Berardinis