Cam crack failures are a common occurrence in cam-follower systems often caused by excessive loading or inappropriate operating conditions. An investigation into such a failure was conducted to assess the effect of cam crack damage on the dynamic behavior of cam-follower systems. It was shown both theoretically and experimentally that a cracked cam causes an overall reduction in stiffness. To further probe the effect, investigators derived an analytical formula expressing the time varying stiffness of a cam-follower system. They also succeeded in quantifying the relationship between crack size and stiffness, showing that cracks have an amplitude modulating effect.

You do not currently have access to this chapter.
Don't already have an account? Register

M. Tounsi, M.S. Abbes, T. Fakhfakh, M. Haddar, 2019. "Failure Analysis of a Cam–Follower System Affected by a Crack", Handbook of Case Histories in Failure Analysis, Larry Berardinis

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal