The various types of stainless steel have very different deformation characteristics in terms of strain hardening and anisotropy. It is important to understand and exploit these characteristics to optimize forming of stainless steels. This chapter discusses the various deformation processes involved in sheet-forming techniques, namely stretch forming and deep drawing. In addition, it provides information on some of the factors pertinent to cold-heading and hot forming of stainless long products.