This chapter deals with corrosion kinetics, which allows the readers to understand the rates of corrosion. The discussion covers two kinetic processes, namely electrode reactions at the cathode and anode and conduction of ions in the electrolyte and provides information on passivation and its effect on polarization diagrams.