Abstract

This appendix contains a temperature conversion table listing the temperature readings (deg For deg C) to be converted into equivalent Fahrenheit or Celsius values. It also contains tables listing equivalent hardness numbers and tensile strengths for Vickers hardness numbers for steel and factors for conversion to SI units.