This chapter discusses various alloying and processing approaches to increase the strength of low-carbon steels. It describes hot-rolled low-carbon steels, cold-rolled and annealed low-carbon steels, interstitial-free or ultra-low carbon steels, high-strength, low-alloy (HSLA) steels, dual-phase (DP) steels, transformation-induced plasticity (TRIP) steels, and martensitic low-carbon steels. It also discusses twinning-induced plasticity (TWIP) steels along with quenched and partitioned (Q&P) steels.

You do not currently have access to this chapter.
Don't already have an account? Register

2015. "Low-Carbon Steels", Steels: Processing, Structure, and Performance, George Krauss