The formation of martensite is characterized by its athermal transformation kinetics, crystallographic features, and development of fine structure. This chapter describes the diffusionless, shear-type transformation of austenite to martensite and how it affects the morphology and microstructure of heat-treatable carbon steels. It also provides information on lath and plate martensite and how they differ in structure and deformation properties.

You do not currently have access to this chapter.
Don't already have an account? Register

2015. "Martensite", Steels: Processing, Structure, and Performance, George Krauss