Skip to Main Content

Abstract

ASTM and other standards organizations have developed a number of tests for evaluating stress-corrosion cracking (SCC) under various conditions. This appendix lists many of the SCC tests that have been approved for specific materials and operating environments.

You do not currently have access to this chapter.
Don't already have an account? Register

2017. "Stress Corrosion Testing Methods and Standards", Stress-Corrosion Cracking: Materials Performance and Evaluation, Russell H. Jones