This article discusses the techniques and applications of synchrotron x-ray diffraction, providing information on x-ray generation, monochromation, and crystallography. X-ray diffraction techniques covered include single-crystal and powder diffraction. Some of the factors involved in the construction and development of macromolecular x-ray crystallography are also described.
Wenqian Xu, Saul H. Lapidus, Andrey Y. Yakovenko, Youngchang Kim, Olaf J. Borkiewicz, Kamila M. Wiaderek, Yu-Sheng Chen, Tiffany L. Kinnibrugh, Synchrotron X-Ray Diffraction Applications, Materials Characterization, Vol 10, 2019 ed., ASM Handbook, ASM International, 2019, p 478–491, https://doi.org/10.31399/asm.hb.v10.a0006654