The response of titanium and titanium alloys to heat treatment depends on the composition of the metal, the effects of the alloying elements on the alpha-beta crystal transformation, and the thermomechanical processing utilized during processing of the alloy. This article provides a detailed discussion on the effects of heat treatment on the mechanical properties for three general classes of titanium alloys, namely, alpha and near-alpha titanium alloys, alpha-beta alloys, and beta alloys.

You do not currently have access to this chapter.
Don't already have an account? Register

Rodney R. Boyer, John Foltz, 2016. "Effect of Heat Treatment on Mechanical Properties of Titanium Alloys", Heat Treating of Nonferrous Alloys, George E. Totten