Quenching refers to the rapid cooling of metal from the solution treating temperature, typically between 465 and 565 deg C (870 and 1050 deg F) for aluminum alloys. This article provides an overview on the appropriate quenching process and factors used to determine suitable cooling rate. It describes the quench sensitivity and severity of alloys, quench mechanisms and the different types of quenchants used in immersion, spray, and fog quenching. The article provides a detailed description of the quench-factor analysis that mainly includes residual stress and distortion, which can be controlled by proper racking. It concludes with information on agitation and the quench tank system used in the quenching of aluminum alloys.

You do not currently have access to this chapter.
Don't already have an account? Register

D. Scott MacKenzie, Niels Bogh, Tom Croucher, 2016. "Quenching of Aluminum Alloys", Heat Treating of Nonferrous Alloys, George E. Totten

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal