Modeling and Simulation of Microstructure Evolution during Heat Treatment of Titanium Alloys

By
Rongpei Shi
Rongpei Shi
The Ohio State University
Search for other works by this author on:
;
Yunzhi Wang
Yunzhi Wang
The Ohio State University
Search for other works by this author on:
;
Dong Wang
Dong Wang
The Ohio State University and Xi‘an Jiaotong University
Search for other works by this author on:
Published:
2016
Page range:
573 - 603
Publication history
November 11, 2016

Abstract

This article describes the integration of thermodynamic modeling, mobility database, and phase-transformation crystallography into phase-field modeling and its combination with transformation texture modeling to predict phase equilibrium, phase transformation, microstructure evolution, and transformation texture development during heat treatment of multicomponent alpha/beta and beta titanium alloys. It includes quantitative description of Burgers orientation relationship and path, discussion of lattice correspondence between the alpha and beta phases, and determination of the total number of Burgers correspondence variants and orientation variants. The article also includes calculation of the transformation strain with contributions from defect structures developed at alpha/beta interfaces as a precipitates grow in size. In the CALculation of PHAse Diagram (CALPHAD) framework, the Gibbs free energies and atomic mobilities are established as functions of temperature, pressure, and composition and serve directly as key inputs of any microstructure modeling. The article presents examples of the integrated computation tool set in simulating microstructural evolution.

You do not currently have access to this content.
Don't already have an account? Register

Rongpei Shi, Yunzhi Wang, Dong Wang, 2016. "Modeling and Simulation of Microstructure Evolution during Heat Treatment of Titanium Alloys", Heat Treating of Nonferrous Alloys, George E. Totten

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal