This article discusses the various methods for evaluating the quench sensitivity of aluminum alloys, namely, time-temperature-property diagrams, the quench factor analysis, the Jominy end-quench method, and continuous-cooling precipitation diagrams. It briefly describes the procedures, applications, advantages, and limitations of these methods.

You do not currently have access to this chapter.
Don't already have an account? Register

2016. "Quench Sensitivity of Aluminum Alloys", Heat Treating of Nonferrous Alloys, George E. Totten