This article describes the annealing behavior of precious metals, namely, gold, silver, platinum, palladium, iridium, rhodium, ruthenium, and osmium. It discusses the annealing practices and their effect on the basic properties of common precious metal alloys. The article presents the typical properties and compositions of silver-copper alloys and gold jewelry alloys such as colored gold alloys and white gold alloys.

You do not currently have access to this chapter.
Don't already have an account? Register

Grigory Raykhtsaum, 2016. "Annealing of Precious Metals", Heat Treating of Nonferrous Alloys, George E. Totten