1-4 of 4 Search Results for

woven fabrics

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001032
EISBN: 978-1-62708-214-3
...Abstract Abstract A Stirling engine heat pipe failed after only 2h of operation in a test situation. Cracking at the leading edge of an evaporator fin allowed air to enter the system and react with the sodium coolant. The fin was fabricated from 0.8 mm (0.03 in.) thick Inconel 600 sheet...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003532
EISBN: 978-1-62708-180-1
... cooled 27 (6) 240–300Comp Until plane Silk cloth 9 μm polycrystalline diamond suspension 27 (6) 120–150Comp 5 Synthetic woven cloth 3 μm polycrystalline diamond suspension 27 (6) 120–150Comp 4 Synthetic short nap cloth ∼0.05 μm colloidal silica or sol-gel alumina suspensions 27 (6...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006765
EISBN: 978-1-62708-295-2
..., and etching. The influence of microstructures on the failure of a material is discussed and examples of such work are given to illustrate the value of light microscopy. In addition, information on heat-treatment-related failures, fabrication-/machining-related failures, and service failures is provided...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001033
EISBN: 978-1-62708-214-3
... 200-mesh woven screens with 41 µm (1600 µin.) diam wires ( Fig. 2 ). These screens were pressed into the annular space at the base of the heater ( Fig. 3 ), which was located between the displacer cylinder and the heater housing. Fig. 2 Stack of 350 type 304 stainless steel regenerator screens...