1-5 of 5 Search Results for

waste incineration

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001046
EISBN: 978-1-62708-214-3
... 825 −1.53 −127.34 −8.52 −25.89 XRD analysis of spelled corrosion scales from various high-temperature alloys exposed to a simulated waste incinerator environment Table 4 XRD analysis of spelled corrosion scales from various high-temperature alloys exposed to a simulated waste...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003555
EISBN: 978-1-62708-180-1
... composition, time, and gas composition. High-temperature corrosive environments may include power-generation plants (coal, oil, natural gas, and nuclear), pulp and paper mills, waste incineration sites, numerous industrial chemical processes, diesel engines (power, land vehicle, and maritime), and gas turbine...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.usage.c0091756
EISBN: 978-1-62708-236-5
.... Abstract Abstract An alloy IN-690 (N06690) incinerator liner approximately 0.8 mm (0.031 in.) thick failed after only 250 h of service burning solid waste. Investigation supported the conclusion that the root cause of the failure was overfiring during startup and sulfidation of the nickel-base alloy...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
...-generation plants (coal, oil, natural gas, and nuclear), pulp and paper mills, waste-incineration sites, numerous industrial chemical processes, diesel engines (power, land vehicle, and maritime), and gas turbine (land-based, marine shipboard, and aircraft). Predicting corrosion of metals and alloys...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001834
EISBN: 978-1-62708-241-9
... – 1029 ( 2009 ) 10.1016/j.corsci.2009.02.025 15. French D.N. , Metallurgical Failures in Fossil Fired Boilers ( Wiley , New York , 2000 ) 16. Kawahara Y. , High temperature corrosion mechanisms and effect of alloying elements for materials used in waste incineration...