Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0046044
EISBN: 978-1-62708-235-8
... Abstract A rocket-motor case made of consumable-electrode vacuum arc remelted D-6ac alloy steel failed during hydrostatic proof-pressure testing. Close visual examination, magnetic-particle inspection, and hardness tests showed cracks that appeared to have occurred after austenitizing...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001752
EISBN: 978-1-62708-241-9
... Abstract Results of failure analyses of two aircraft crankshafts are described. These crankshafts were forged from AMS 6414 (similar composition to AISI 4340) vacuum arc remelted steels with sulfur contents of 0.003% (low sulfur) and 0.0005% (ultra-low sulfur). A grain boundary sulfide...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001077
EISBN: 978-1-62708-214-3
... in a region depleted of chromium and nickel. This condition coincides with a microstructural inhomogeneity consisting of large, soft ferrite grains. Its origin was probably contamination of the solidifying ingot during the consumable vacuum arc remelting operation. Bevel gears Forgings Gear teeth...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006792
EISBN: 978-1-62708-295-2
..., elimination of these inclusions during casting leads to an improvement of RCF life and thereby bearing life. Vacuum induction melting, vacuum arc remelting, electroslag remelting, and combinations of these processes are commonly used to produce bearings for demanding applications. Vacuum Induction Melting...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c0047010
EISBN: 978-1-62708-234-1
... or arc remelted or both) in sizes equal to that of the 81-mm mortar tube. Transverse disks cut from each bar were machined into three tensile and two V-notch Charpy specimens for each test condition. For the elevated-temperature tests, tensile-test bars were pulled after being held at temperature...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003509
EISBN: 978-1-62708-180-1
... imperfections may be tolerable and how the other may be root-cause defects in service failures. The article explains the effects of joint design on weldment integrity. It outlines the origins of failure associated with the inherent discontinuity of welds and the imperfections that might be introduced from arc...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006808
EISBN: 978-1-62708-329-4
... of arc welds. Mechanical and environmental failure origins related to other types of welding processes are also described. The article explains the cause and effects of process-related discontinuities including weld porosity, inclusions, incomplete fusion, and incomplete penetration. Different fitness...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006864
EISBN: 978-1-62708-395-9
... of an immiscible polymer blend. A vacuum is often applied to aid in the removal of moisture/volatiles and degradation products. Finally, the degassing operation can be used to dry hygroscopic polymers during the extrusion process. Caution must be used in this case so that the polymer in question does not degrade...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001810
EISBN: 978-1-62708-180-1
...) or vacuum arc remelting (VAR). However, steel from these secondary refining processes is still required for bearings in high-reliability applications, such as aircraft engines. The bearing industry has used through-hardened material, such as 52100, for ball bearings since early introduction in Europe...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001808
EISBN: 978-1-62708-180-1
..., weld defects, or arc strikes. Occasionally, brittle fractures are encountered, particularly in low-temperature environments or as a result of impact or a rapidly applied overload. Brittle fracture may thus be attributable to inappropriate choice of material because of incomplete knowledge...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003532
EISBN: 978-1-62708-180-1
... resins, although more expensive than acrylics, are commonly used in failure studies, because epoxy physically adheres to specimens and can be drawn into cracks and pores, particularly if a vacuum impregnation chamber is employed and a low viscosity epoxy is used. Epoxies are very suitable for mounting...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006810
EISBN: 978-1-62708-329-4
..., gross nonmetallic inclusions, brittle second-phase particles, weld defects, or arc strikes. Occasionally, brittle fractures are encountered, particularly in low-temperature environments or as a result of impact or a rapidly applied overload. Brittle fracture may thus be attributable to inappropriate...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959
EISBN: 978-1-62708-395-9
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006765
EISBN: 978-1-62708-295-2
... studies, because shrinkage is a problem with acrylics. Epoxy resins, although more expensive than acrylics, are commonly used in failure studies, because epoxy physically adheres to specimens and can be drawn into cracks and pores, particularly if a vacuum-impregnation chamber is employed and a low...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001814
EISBN: 978-1-62708-180-1
... in tension, and such data are available for both room temperature and elevated temperatures. Tension, compression, and hardness testing arc discussed in separate articles in Volume 8 of ASM Handbook , formerly 9th Edition Metals Handbook. As a class, tool steels are not noted for high toughness...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006834
EISBN: 978-1-62708-329-4
... (WN 1.4108 or AMS 5898), that exhibit exceptional corrosion resistance under various corrosive environments. These steels, obtained by pressurized electroslag remelting processes, are enriched in nitrogen, have a very high degree of purity, and present very fine microdispersed carbonitride carbides (6...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006779
EISBN: 978-1-62708-295-2
...., Gauss, Weibull, logit, arc sin p ) and the failure probability. Table 2 shows u -values for different failure probabilities for the most often applied Gauss log distribution. Safety span for different failure probabilities (Gauss log distribution) Table 2 Safety span for different...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003544
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006831
EISBN: 978-1-62708-329-4
... for applications requiring wear resistance. Gray Iron Processing Cupolas, induction furnaces (both coreless and channel induction furnaces), and arc furnaces are used to prepare the molten state required for processing gray cast iron. The economics of the particular situation is the principal factor used...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.9781627083294
EISBN: 978-1-62708-329-4