Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001105
EISBN: 978-1-62708-214-3
... and secondary microcracks. 150×. Abstract A tie rod, nut, and bellows from a failed 610 mm (24 in.) diam tied universal expansion joint that carried tail gases consisting of N 2 + O 2 with slight traces of nitrogen oxides and water were examined. The materials were SA 193-B7 (AISI 4140), SA 194–214...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c0048592
EISBN: 978-1-62708-218-1
... of four bearing caps, two cap screws, and one universal-joint spider had fractured. Examination of the three fractured bearing caps and the spider showed no evidence of fatigue but showed that fracture occurred in a brittle manner. The bearing cap that was not destroyed still contained portions of the two...
Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001271
EISBN: 978-1-62708-215-0
... eye. Failure occurred when two hammers were struck together during an attempt to free a universal joint from an automotive drive shaft. Two samples were cut from the face of the hammer one through the chipped area on the chamfer and the other from the undamaged area on the chamfer. The shape...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c0089543
EISBN: 978-1-62708-226-6
.... Wallace, Case Western Reserve University; Charles F. Walton, professional engineer; Peter F. Wieser, Case Western Reserve University; Frank J. Worzala, University of Wisconsin; Carl J. Czajkowski, Department of Nuclear Energy, Brookhaven National Laboratory, Upton, New York; and Mohan D. Chaudhari...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.pulp.c0089682
EISBN: 978-1-62708-230-3
.... Goodrich, Taussig Associates, Inc.; Renita G. King, Cummins Engine Company; Dilip K. Subramanyam, Abex Corporation; John F. Wallace, Case Western Reserve University; Charles F. Walton, professional engineer; Peter F. Wieser, Case Western Reserve University; Frank J. Worzala, University of Wisconsin; Carl J...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c0089563
EISBN: 978-1-62708-217-4
..., Navistar International, Inc.; George M. Goodrich, Taussig Associates, Inc.; Renita G. King, Cummins Engine Company; Dilip K. Subramanyam, Abex Corporation; John F. Wallace, Case Western Reserve University; Charles F. Walton, professional engineer; Peter F. Wieser, Case Western Reserve University; Frank J...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.rail.c0047328
EISBN: 978-1-62708-231-0
... The following contributors provided case histories or other useful information: Charles O. Cambridge, Navistar International, Inc.; George M. Goodrich, Taussig Associates, Inc.; Renita G. King, Cummins Engine Company; Dilip K. Subramanyam, Abex Corporation; John F. Wallace, Case Western Reserve University...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.bldgs.c0089530
EISBN: 978-1-62708-219-8
... Reserve University; Charles F. Walton, professional engineer; Peter F. Wieser, Case Western Reserve University; Frank J. Worzala, University of Wisconsin; Carl J. Czajkowski, Department of Nuclear Energy, Brookhaven National Laboratory, Upton, New York; and Mohan D. Chaudhari, Columbus Metallurgical...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c0089551
EISBN: 978-1-62708-218-1
... histories or other useful information to the source article: Charles O. Cambridge, Navistar International, Inc.; George M. Goodrich, Taussig Associates, Inc.; Renita G. King, Cummins Engine Company; Dilip K. Subramanyam, Abex Corporation; John F. Wallace, Case Western Reserve University; Charles F. Walton...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.chem.c0089633
EISBN: 978-1-62708-220-4
... Reserve University; Charles F. Walton, professional engineer; Peter F. Wieser, Case Western Reserve University; Frank J. Worzala, University of Wisconsin; Carl J. Czajkowski, Department of Nuclear Energy, Brookhaven National Laboratory, Upton, New York; and Mohan D. Chaudhari, Columbus Metallurgical...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.machtools.c0089534
EISBN: 978-1-62708-223-5
..., Cummins Engine Company; Dilip K. Subramanyam, Abex Corporation; John F. Wallace, Case Western Reserve University; Charles F. Walton, professional engineer; Peter F. Wieser, Case Western Reserve University; Frank J. Worzala, University of Wisconsin; Carl J. Czajkowski, Department of Nuclear Energy...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.power.c0089663
EISBN: 978-1-62708-229-7
...: Charles O. Cambridge, Navistar International, Inc.; George M. Goodrich, Taussig Associates, Inc.; Renita G. King, Cummins Engine Company; Dilip K. Subramanyam, Abex Corporation; John F. Wallace, Case Western Reserve University; Charles F. Walton, professional engineer; Peter F. Wieser, Case Western...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0089651
EISBN: 978-1-62708-235-8
.... Wallace, Case Western Reserve University; Charles F. Walton, professional engineer; Peter F. Wieser, Case Western Reserve University; Frank J. Worzala, University of Wisconsin; Carl J. Czajkowski, Department of Nuclear Energy, Brookhaven National Laboratory, Upton, New York; and Mohan D. Chaudhari...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001764
EISBN: 978-1-62708-241-9
... on a component surface through a single node off the component surface, as indicated in the figure. In the present case, the MPCs model the point of load transfer to the component of interest, which occurs in the cross of the universal joint. The level of torque selected for the analysis does not, in any way...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.process.c0089646
EISBN: 978-1-62708-235-8
... Associates, Inc.; Renita G. King, Cummins Engine Company; Dilip K. Subramanyam, Abex Corporation; John F. Wallace, Case Western Reserve University; Charles F. Walton, professional engineer; Peter F. Wieser, Case Western Reserve University; Frank J. Worzala, University of Wisconsin; Carl J. Czajkowski...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c0089572
EISBN: 978-1-62708-218-1
..., Abex Corporation; John F. Wallace, Case Western Reserve University; Charles F. Walton, professional engineer; Peter F. Wieser, Case Western Reserve University; Frank J. Worzala, University of Wisconsin; Carl J. Czajkowski, Department of Nuclear Energy, Brookhaven National Laboratory, Upton, New York...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001405
EISBN: 978-1-62708-234-1
... of the pearlite grains, and was observed independently in the Company's Research Dept. and by Dr. C. D. Weir, of Glasgow University, at about the same time. This feature has been looked for and found in every case of caustic cracking that has been investigated, and in several instances its absence has served...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.pulp.c0089567
EISBN: 978-1-62708-230-3
..., Inc.; Renita G. King, Cummins Engine Company; Dilip K. Subramanyam, Abex Corporation; John F. Wallace, Case Western Reserve University; Charles F. Walton, professional engineer; Peter F. Wieser, Case Western Reserve University; Frank J. Worzala, University of Wisconsin; Carl J. Czajkowski, Department...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.matlhand.c0089676
EISBN: 978-1-62708-224-2
.... Cambridge, Navistar International, Inc.; George M. Goodrich, Taussig Associates, Inc.; Renita G. King, Cummins Engine Company; Dilip K. Subramanyam, Abex Corporation; John F. Wallace, Case Western Reserve University; Charles F. Walton, professional engineer; Peter F. Wieser, Case Western Reserve University...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.steel.c0089617
EISBN: 978-1-62708-232-7
... provided case histories or other useful information to the source article: Charles O. Cambridge, Navistar International, Inc.; George M. Goodrich, Taussig Associates, Inc.; Renita G. King, Cummins Engine Company; Dilip K. Subramanyam, Abex Corporation; John F. Wallace, Case Western Reserve University...