Series: ASM Failure Analysis Case Histories
Volume: 2
Publisher: ASM International
Published: 01 December 1993
DOI: 10.31399/asm.fach.v02.c9001291
EISBN: 978-1-62708-215-0
... for fatigue crack growth during service. It was recommended that the damaged undercarriage struts be withdrawn from service pending further analysis and development of a repair technique. Crack propagation Military planes 35NCD16 Surface treatment related failures Intergranular fracture Fatigue...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.aero.c9001744
EISBN: 978-1-62708-217-4
... Abstract Two examples involved brittle fracture promoted by small fatigue cracks owing to welding deficiencies. Other parts involving inadequate welding were a ski-wheel axle flange, ski fitting (brackets), and undercarriage shock strut stub assembly. In an attach fitting for an engine mount...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001020
EISBN: 978-1-62708-214-3
... . Fig. 1 General configuration of main landing gear undercarriage. Fig. 2 Main landing gear components. Shock (or oleo) struts are self-contained hydraulic units that use compressed air combined with hydraulic fluid to absorb and dissipate their imposed loads. Each shock strut...