EISBN: 978-1-62708-180-1
... to control corrosion of the structure as well as provide structural integrity where leaks exist. Properly selected and applied high-performance epoxy can protect H 2 S headspace corrosion on wastewater treatment facilities and related structures. The spray-on or trowel-on high-performance structural epoxy...