1-20 of 77 Search Results for

transmission system

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.conag.c9001248
EISBN: 978-1-62708-221-1
...Abstract Abstract Failure occurred in the teeth of a case-hardening Ni-Cr-Mo alloy steel spur gear in the transmission system of heavy duty tracked vehicles. The defects were in the nature of seizure on the involute profile. Scrutiny of the transmission system showed there might be choking...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001763
EISBN: 978-1-62708-241-9
...Abstract Abstract This paper presents a failure analysis of a reverse shaft in the transmission system of an all-terrain vehicle (ATV). The reverse shaft with splines fractured into two pieces during operation. Visual examination of the fractured surface clearly showed cracks initiated from...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.modes.c9001681
EISBN: 978-1-62708-234-1
...). To assist in this procedure, a microstructural analysis was made of the cast components. This involved optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscopy (TEM) and scanning transmission electron microscopy (STEM). IN SEM and STEM, microchemical analyses were...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001768
EISBN: 978-1-62708-241-9
...Abstract Abstract A steel splice plate in a power transmission line tower cracked while in service. Metallographic analysis indicated the presence of a white hard martensite layer near the crack, which occurred in the heel of the plate. Mechanical property tests revealed localized hardening...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.auto.c0047846
EISBN: 978-1-62708-218-1
... from shock loading. It was revealed by visual examination that the fracture had initiated in the sharp corner at the bottom of a longitudinal hole which was part of a force feed lubricating system. Beach marks were observed on the fracture surfaces. It was revealed by further examination that the slip...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006764
EISBN: 978-1-62708-295-2
... and cracks, while methods such as radiography and ultrasound are capable of detecting imperfections within a part. Other methods are more suited for online monitoring, which is a quality-control function in production systems. Also, there are many NDE methods used for condition monitoring of parts in service...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001076
EISBN: 978-1-62708-214-3
... turbine operating at a gas transmission installation. Visual Macrophotography Microstructural Analysis Corrosion Morphology Material The EDS attack was probably caused by electrical current within the system. Such currents may result from residual magnetism from welding or from magnetic...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001766
EISBN: 978-1-62708-241-9
...Abstract Abstract During the installation of power transmission lines across a major interstate highway, a temporary anchor stabilizing one of the poles failed, resulting in the loss of the pole and the associated power lines. It also contributed to a single vehicle incident on the adjacent...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001800
EISBN: 978-1-62708-241-9
... . 10.31399/asm.hb.v19.a0002377 Multiple in-service fractures of torsion springs were experienced in the same system, which was the support assembly to the electrical pickup for an electric-powered vehicle, similar to a subway rail car or electric trolley car. The remainder of the system details...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001031
EISBN: 978-1-62708-214-3
... s. This was significantly less than the average lifetime of approximately 30,000 s. An MCC is retired from service when the hydrogen coolant loss is greater than the engine system balance can accommodate. Specimen locations were selected to determine the nature and extent of material degradation...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001792
EISBN: 978-1-62708-241-9
... to the propeller, is made of low alloy steel. The other shaft, part of a clutch mechanism that regulates the transmission of power from the engine to the gears, is made of carbon steel. Fracture surface examination of the gear shaft revealed circumferential ratchet marks with the presence of inward progressive...
Series: ASM Failure Analysis Case Histories
Volume: 1
Publisher: ASM International
Published: 01 December 1992
DOI: 10.31399/asm.fach.v01.c9001024
EISBN: 978-1-62708-214-3
...Abstract Abstract A Marine Corps helicopter crash was investigated. Efforts were directed to the failure of one of the main rotor blades that had apparently separated in the air. The apparent failure of a blade integrity monitor (BIM) system was also considered. The rotor blade comprised a long...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006762
EISBN: 978-1-62708-295-2
... of the communication method requested, documentation of the work should be generated. It is recommended that the investigator discuss what level of security is required for transmitting the information. For example, should e-mails, correspondence, updates, and reports be encrypted? For electronic transmission...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001820
EISBN: 978-1-62708-180-1
..., transmission lines, and distribution lines. Gas or crude oil gathering lines exist between a well and a treatment plant or collection point. These are usually relatively small-diameter lines (51 to 203 mm, or 2 to 8 in., in diameter) and operate at a variety of pressures, usually from 3490 to 8376 kPa (500...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001799
EISBN: 978-1-62708-241-9
...Abstract Abstract A high-speed pinion gear shaft, part of a system that compresses natural gas, was analyzed to determine why it failed. An abnormal wear pattern was observed on the shaft surface beneath the inner race of the support bearings. Material from the shaft had transferred...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003523
EISBN: 978-1-62708-180-1
... into a guy wire of a power transmission pole Analytical/mathematical models give a representation of physical system or process in a different manner. These models are based on mathematical equations and are intended to be deterministic or predictive of the outcome of an event or process...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001775
EISBN: 978-1-62708-241-9
... is inverted and the line is filled with caustic solution. In addition, during shutdown operations atmospheric air enters the system. This air is routinely removed by steaming prior to system restart. Fig. 1 The bent tube that failed during service. Cracking appeared in the missing part of the tube...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006766
EISBN: 978-1-62708-295-2
... Fig. 2 Schematic diagram of inductively coupled plasma optical emission spectroscopy system. RF, radio frequency. Source: Ref 3 Fig. 1 Schematic of spark emission spectroscopy system. Source: Ref 1 Abstract Identification of alloys using quantitative chemical analysis...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006774
EISBN: 978-1-62708-295-2
... of the physical evidence. Magnitude and direction of loading, interaction with other components, damage sequencing in systems, and other valuable information may be reliant upon the investigation and reconstruction of fracture patterns. In this way, inspection and analysis of fracture surfaces may be critical...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.9781627081801
EISBN: 978-1-62708-180-1