Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006788
EISBN: 978-1-62708-295-2
... collection in the identification of microbiologically influenced corrosion in a field corrosion site. XRD, x-ray diffraction; EDX, energy-dispersive x-ray analysis; ATP, adenosine triphosphate; MPN, most probable number; MMM, molecular microbiological methods; APS, adenosine-5′-phosphosulfate. Adapted from...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003556
EISBN: 978-1-62708-180-1
... to the test solution after buffering with excess sodium acetate yields a white precipitate if calcium is present. These qualitative chemical assays have been made available commercially in the form of a test kit through the GRI program noted previously. X-ray diffraction (XRD) analysis of crystalline material...