Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001819
EISBN: 978-1-62708-180-1
..., and degradation. Finally, the article discusses the fatigue properties of implant materials and the fractures of total hip joint prostheses. degradation fatigue properties fractures implant deficiencies internal fixation devices orthopedic implants prosthetic implants total hip joint prostheses...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001664
EISBN: 978-1-62708-226-6
... – 48 ( 1972 ). 3. Galante J. O. , Rostoker W. and Doyle J. M. , “Failed Femoral Stems in Total Hip Prostheses,” The Journal of Bone and Joint Surgery , Vol. 57A , pp. 230 – 236 ( 1975 ). 4. Gilbertson L. N. , “The Relationship in Microstructure to Fracture...
Series: ASM Failure Analysis Case Histories
Volume: 3
Publisher: ASM International
Published: 01 December 2019
DOI: 10.31399/asm.fach.v03.c9001803
EISBN: 978-1-62708-241-9
... Composite Femoral Prostheses for Total Hip Arthroplasty ,” Biomaterials , 2002 , 23 , pp. 4249 – 4262 . 10.1016/S0142-9612(02)00188-6 16. Jaffe W.L. and Scott D.F. : “ Total Hip Arthroplasty with Hydroxyapatite-Coated Prosthesis ,” J. Bone Joint Surg. , 1996 , 78 – A(12) , pp...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003571
EISBN: 978-1-62708-180-1
... of Ultra-High Molecular Weight Polyethylene in Total Joint Replacements , New Directions in Tribology , Hutchings I. , Ed., Mechanical Engineering Publications Ltd. , London , 1997 , p 443 – 458 45. Unsworth A. , The Effects of Lubrication in Hip Joint Prostheses , Phys. Med. Biol...
Series: ASM Failure Analysis Case Histories
Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.med.c9001690
EISBN: 978-1-62708-226-6
... to functional surfaces, such as the fracture surface of broken implants and bearing surfaces of joint prostheses. 10 , 11 , 12 , 13 , 14 The clinical history of the implant and the medical history of the patient (reasons for insertion, additional diagnoses, and complications) are important sources...