Publisher: ASM International
Published: 01 June 2019
DOI: 10.31399/asm.fach.pulp.c0045911
EISBN: 978-1-62708-230-3
...) and 420 °C (790 °F). Each bellows was of a three-ply design; each ply contained two longitudinal gas tungsten arc welds and was cold formed with 13 convolutions. The welds had been inspected with dye penetrant. The Inconel 600 had been received as 1.5-mm (0.060-in.) thick sheets, hot rolled to final...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006936
EISBN: 978-1-62708-395-9
... to detection and characterization. This article focuses on the three common methods for ultrasonic nondestructive inspection of plastics, namely pitch-catch, through-transmission, and pulse-echo, as well as the three basic types of ultrasonic NDE scans: the A-scan, B-scan, and C-scan. The discussion includes...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006932
EISBN: 978-1-62708-395-9
... materials has necessitated increasing the body of knowledge on this subject. Some excellent reviews in this area are available in the literature ( Ref 2 - 4 ). There are three types of internal stresses in amorphous polymers (this classification scheme can be extended to include semicrystalline polymers...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006916
EISBN: 978-1-62708-395-9
... and orientation. It also presents examples of failures stemming from material degradation improper use of metal inserts, weak weld lines, insufficient curing of thermosets, and inadequate mixing and impregnation in the case of thermoset composites. injection molding manufacturing-related failures...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006924
EISBN: 978-1-62708-395-9
... group (three-member ring on the left) reacts with the nitrogen on the primary amine (nitrogen-containing molecule) to open the epoxy group and link these moieties together. The nitrogen at the end of the growing molecule can subsequently react with another epoxy group. The molecular weight increases...