EISBN: 978-1-62708-180-1
..., wear study is separated as elastomers, thermosets, glassy thermoplastics, and semicrystalline thermoplastics. The article describes the effects of environment and lubricant on the wear failures of polymers. It presents a case study on nylon as a tribological material. The article explains the wear...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006850
EISBN: 978-1-62708-395-9
..., but no material is actually removed. (e) A typical friction/scratching force profile when a slider is passed over an elastomer. Reprinted with permission from Ref 1 . Thermosets Thermosets have found applications mainly in automobile brakes, gears, cams, and clutch parts, where they are subjected...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006925
EISBN: 978-1-62708-395-9
... polymer molecule. Thermoplastic materials often melt upon heating but return to their original solid condition when cooled. In contrast, thermosets are invariably composed of some type of three-dimensional cross linking of polymer chains. The cross linking of thermoset plastics often involves primary...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006864
EISBN: 978-1-62708-395-9
... Applications and Typical Products In the simplest terms, all plastics processing techniques involve three key steps: fluidizing (plasticating), shaping, and solidification. Raw materials are typically sourced as pellets or powders (thermoplastic) or as monomeric liquid and cross-linking agent (thermoset...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.9781627083959
EISBN: 978-1-62708-395-9
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006765
EISBN: 978-1-62708-295-2
... sources of injurious effects. The most common mounting method uses a device, called a mounting press, to provide the required pressure and heat to encapsulate the specimen with a thermosetting or thermoplastic mounting material. Common thermosetting resins include phenolic, diallyl phthalate...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006931
EISBN: 978-1-62708-395-9
... of the material. Wide-angle x-ray diffraction, as well as electron microscopy, can determine the morphology, or structure (amorphous or crystalline), of the material. This problem-solving approach can be extended from failed pipe to a polymeric structural member that failed under load, or a plastic gear...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003572
EISBN: 978-1-62708-180-1
... composites (SFRP and particulate-filled), unidirectional FRP composites, and fabric reinforced composites. Friction and wear performance of the composites, correlation of performance with various materials properties, and studies on wear-of failure mechanisms by scanning electron microscopy are discussed...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006870
EISBN: 978-1-62708-395-9
...-twentieth century, the typical materials involved in fractography were metals, ceramics, and glass. In recent decades, efforts have grown to include thermoplastics ( Ref 2 ) and thermosets (such as rubber) with an emphasis on the similarities between thermoplastics and metals. In this article, I examine...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003522
EISBN: 978-1-62708-180-1
... Abstract This article focuses on the visual or macroscopic examination of damaged materials and interpretation of damage and fracture features. Analytical tools available for evaluations of corrosion and wear damage features include energy dispersive spectroscopy, electron probe microanalysis...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006757
EISBN: 978-1-62708-295-2
..., for typical types of damage experienced for metallic components. This article discusses the processes involved in visual or macroscopic examination of damaged material; the interpretation of fracture features, corrosion, and wear damage features; and the analysis of base material composition. It covers...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006915
EISBN: 978-1-62708-395-9
..., and medical devices. Often they are more dimensionally stable and have use temperatures above 130 °C (265 °F). They tend to be more durable and also more expensive, up to many times the cost of the commodity materials. However, the definitions allow for some overlap between the categories ( Ref 1...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006800
EISBN: 978-1-62708-329-4
... options to a broad category of material. Metals can be subdivided into categories such as carbon steel, stainless steel, and copper alloys. Plastics can be subdivided into specific classes of thermoplastics and thermosets, such as polycarbonates and polyesters. Level IV: Select a specific material...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003501
EISBN: 978-1-62708-180-1
... category of material. Metals can be subdivided into categories such as carbon steel, stainless steel, and copper alloys. Plastics can be subdivided into specific classes of thermoplastics and thermosets, such as polycarbonates and polyesters. Level IV: Select a specific material according...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006911
EISBN: 978-1-62708-395-9
... substrate and removes material. These wear mechanisms are important to test when searching for polymers that are resistant to abrasive wear because of their eventual application. Examples of this include the testing of elastomers for car tires, exposed polymer gears, and polymers for joint implants...