..., and unidirectional bending usually produce the beach-mark pattern shown in Fig. 2(j) . Example 1: Unidirectional-Bending Fatigue Failure of an A6 Tool Steel Shaft The shaft shown in Fig. 3 was part of a clamping device on a tooling assembly used for bending 5.7-cm (2.25-in.) outer-diameter tubing on an 8.6...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006797
EISBN: 978-1-62708-295-2
... with a lateral force (upper arrow). Source: Ref 4 . (b) Medium-length tube tested to buckling instability on special-purpose-designed test machine. Source: Ref 3 Fig. 5 Diagram of the temperature dependence of elastic, plastic, and fracture behavior of polycrystalline materials that do not exhibit...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003573
EISBN: 978-1-62708-180-1
... not be permanent deformation, depending on whether or not the yield strength was exceeded. Long, slender, straight bars, tubes, or columns under axial compressive forces will buckle when the buckling load is exceeded. Buckling failure may also be encountered on the compressive sides of tubes, I-beams, channels...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003565
EISBN: 978-1-62708-180-1
... is described as normal impact wear. Where a shear component is added, either when normal impact occurs with a component of sliding or the bodies impact at a tangent, the term compound impact wear is used. Most of the situations described above involve impact with a small amount of sliding. Compound impact...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006793
EISBN: 978-1-62708-295-2
... associated not only with the need for frequent replacement of parts but also in the downtime incurred. Unintentional impacts, such as those arising from the chattering and relative motion of tubes carrying waste from nuclear reactors, can give rise to situations where safety and reliability are of critical...